Загрузка страницы

Lining the Super C Forge

UPDATE UPDATE.... When you light the forge for the final curing of the mortar (before the second layer of slurry), set the burner at a low heat, just enough to keep the burner going with a steady flame.

This video shows how I line the forge I made in the "Build a Super C Propane Forge" video. The lining is INSWOOL thermal blanket with a reflective coating over the blanket. This type of lining costs more to install, but it should be more efficient (faster heating) and economical (less propane usage) than using just thermal blanket lining.

There will be additional videos coming that will provide more details about floors, doors, using propane forges, material sources and a free-form forge (please be patient).

Please, please, please..... obtain the MATERIAL SAFETY DATA SHEETS for the products you use and follow the advice for personal safety. You can find this infomation by googling for it, specifying the product name and MSDS.

Do not have any moving air in your shop when you are working with these type of products if they involve powder. Do not use forced air or a vaccum cleaner (unless it has a HEPA filter). Clean up any spilled materials with damp rags.

Видео Lining the Super C Forge канала David Hammer
Показать
Комментарии отсутствуют
Введите заголовок:

Введите адрес ссылки:

Введите адрес видео с YouTube:

Зарегистрируйтесь или войдите с
Информация о видео
16 января 2013 г. 12:31:17
00:27:11
Яндекс.Метрика